For plastic products, the degree of groovedness of the color of oil injection processing is generally selected above 10, do not choose low gloss matte, because its surface hardness will be relatively low, below 1H, and at the same time, the oil injection processing is not wear-resistant. Generally, the hardness of the paint after drying is above 2H, but when the hardness is too high, the paint will be brittle, so the general surface hardness should not exceed 4H. In […]